What die material and coating means at 32 → 20 mm

For Chromoly 4140 (42CrMo / 40KhM) tube at 32 → 20 mm with a 1.5 mm wall, die material and coating comes down to D2 (SKD11) with a TiAlN coating inserts at 60–62 HRC, re-polished rather than replaced. That single line is the answer; the rest of this page is the arithmetic behind it, so you can check the figure against your own drawing instead of taking it on trust.

The die is the part of the machine that decides part quality and tooling cost per piece. Choosing its steel is a volume decision as much as a metallurgy one.

The three practical choices

D2-class tool steel (X12MF / Cr12MoV) at 58–62 HRC is the default for carbon and alloy steel up to moderate volume. It holds a polished land, regrinds easily, and costs a fraction of carbide. The 3.7 per cent scrap allowance is not padding — it is the pass count and the material talking.

Carbide inserts make sense above roughly 300 000 parts a year or when the abrasive loading is high — scaled tube, or aluminium with oxide inclusions. Coated HSS is a middle option that is rarely worth it for taper dies because the coating wears off the land first. The mill certificate matters more than the grade name: spread inside the standard moves the force by about 7 kN.

Where the money actually goes

Die cost per part is the die price divided by the number of parts between regrinds, multiplied by the number of regrinds the die survives. A die that costs twice as much but lasts three times longer is cheaper, and that arithmetic is done before the purchase order, not after. At this size the die sees 47 kN per bite, which is why the Ø50 class (manual or automatic) is the natural home for the job.

The numbers for this combination

Tube outside diameter32 mm
Small-end diameter20 mm
Wall thickness1.5 mm
Cone length55 mm
Reduction on diameter37.5 per cent
Half angle / included angle6.23° / 12.5°
Yield strength used655 MPa
Forming force, single bite120 kN
Forming force, per bite at 3 passes47 kN
Passes3 passes
Processcold forming
Cycle time12.1 s
Output per 8 h shift1,951 pieces
Tip wall after forming1.90 mm (+26 per cent)
Springback on tip diameter0.095 mm
Ovality at the tip1.9 per cent
Blank length100 mm
Blank weight0.113 kg
Machine classØ50 class (manual or automatic)

Computed for this combination. Confirm the force and the tip wall on a sample before the die is cut.

The blank length assumes you grip 35 mm of straight tube in the collet and trim 10 mm after forming. If your chuck is longer, add it to 100 mm — the cone itself does not change, only the material you pay for.

We keep this cell in the library because buyers ask for it by name: they want to know what a 32 → 20 mm cone in Chromoly 4140 (42CrMo / 40KhM) actually costs before they commit to a die. Everything here is traceable to a machine model on this site.

How Chromoly 4140 (42CrMo / 40KhM) behaves at 37.5 per cent reduction

Supplied usually as quenched and tempered, which is exactly the wrong condition for cold forming. Either form it in the annealed state and harden afterwards, or expect a very narrow process window.

In practice the first thing to change with Chromoly 4140 (42CrMo / 40KhM) is not the die but the lubricant film. 4140 chromoly will form on a marginal film for a hundred pieces and then start picking up on the die — the mark appears long before the dimension moves.

At 37.5 per cent reduction the work-hardening from forming is worth roughly 144 MPa of extra yield at the tip. If your next operation is machining, that is helpful; if it is another forming pass, budget for it.

Small section: 32 → 20 mm

Small sections are dominated by handling, not by force. The die is light, the cycle is short, and the biggest quality risk is ovality from manual loading rather than tonnage.

The 100 mm blank is heavy enough — 0.113 kg — that manual loading sets the pace before the forming stroke does. That is why the cycle sits at 12.1 s rather than the 9.4 s the stroke alone would allow.

Machine class for 32 mm is the Ø50 class (manual or automatic). Going one class up buys stiffness you will not use at this diameter and costs floor space you will miss.

Cost per 1,000 pieces

Metal in the blank0.113 kg, 0.197 USD
Machine time12.1 s, 0.060 USD
Die cost, one set1,305 USD
Die life23,547 pieces
Scrap allowance3.7 per cent
Cost per piece0.33 USD
Cost per 1,000325 USD

The 0.33 USD figure excludes finishing, coating and packing. It is the formed part at the machine, which is the only number that lets you compare two processes fairly.

What to put on the drawing

State the material by standard and grade, not by trade name. Chromoly 4140 (42CrMo / 40KhM) covers a range of yield strength wide enough to move the force by 7 kN, and the die is cut for one point in that range.

Say what happens after forming: machined, welded, coated, or used as formed. The allowance, the stress relief and the surface spec all follow from that one line.

If you cannot state the cone length because the part is defined by a mating component, send the mating component instead. We will derive the cone and tell you what the resulting angle is before quoting.

Frequently asked questions

How do I know the die is worn?

The tip diameter grows and the cone gets a polished ring where the land used to bite. Both are visible before parts go out of tolerance if you measure the first part of each shift.

Can a worn die be repaired?

The land can be re-polished two or three times before the profile moves too far. After that the die is re-cut or replaced.

Does coating a die help on stainless?

A PVD coating reduces pick-up noticeably on 304/316. It is a real improvement, not a sales story, but it does not replace EP lubricant.

Can I substitute a different grade and keep the same die?

Sometimes, and only if the yield strength lands within about ten per cent. Chromoly 4140 (42CrMo / 40KhM) at 655 MPa is the number the die was cut for; a grade at 721 MPa will form but will spring back 0.095 mm or more and the tip will run small. Re-cut or re-lap the die rather than fighting it with the stop.

Is 32 → 20 mm a standard die size?

It is a standard die blank with a custom grind. That keeps the die at 1,305 USD rather than a full custom build, and it is why we can quote a sample in two weeks at this size.