What tooling cost per part means at 60 → 38 mm
Short version for Carbon steel (St37 / Q235B) at 60 → 38 mm: 1,400 USD for the die set, or 0.035 USD per piece across 40,000 pieces. It is worth knowing why before you accept it, because the same three inputs that produce this answer will produce a different one the moment the wall or the grade changes.
Die cost per part is the number that decides whether a taper is economic. It is arithmetic, not negotiation, and it changes completely with volume.
The formula
Die price divided by parts between regrinds, added to regrind cost divided by parts per regrind cycle, times the number of cycles the die survives. A die at 1 500 with 40 000 parts between regrinds and three regrinds is about 0.01 per part. The same die at 5 000 annual volume is 0.30. The mill certificate matters more than the grade name: spread inside the standard moves the force by about 8 kN.
That is why a 500-part order is quoted with tooling as a separate line. It is not a markup, it is the honest allocation of a fixed cost. At this size the die sees 74 kN per bite, which is why the L-120×400 F is the natural home for the job.
Where buyers get surprised
Mandrels, second-pass dies and coating-compatible tooling all add cost that does not appear in the basic die quote. A two-pass process roughly doubles tooling before any machining allowance is considered. Running 2 passes puts the cycle at 12.0 s and the shift output near 1,968 pieces.
The other surprise is material grade. A die for stainless needs different surface treatment, and it wears faster, so cost per part can be three times the carbon-steel figure at identical volume. The tip wall finishes at 3.14 mm, 26 per cent heavier than the 2.5 mm you started with — plan the mating bore around that and not around the blank.
The numbers for this combination
| Tube outside diameter | 60 mm |
| Small-end diameter | 38 mm |
| Wall thickness | 2.5 mm |
| Cone length | 95 mm |
| Reduction on diameter | 36.7 per cent |
| Half angle / included angle | 6.60° / 13.2° |
| Yield strength used | 235 MPa |
| Forming force, single bite | 133 kN |
| Forming force, per bite at 2 passes | 74 kN |
| Passes | 2 passes |
| Process | cold forming |
| Cycle time | 12.0 s |
| Output per 8 h shift | 1,968 pieces |
| Tip wall after forming | 3.14 mm (+26 per cent) |
| Springback on tip diameter | 0.048 mm |
| Ovality at the tip | 1.3 per cent |
| Blank length | 171 mm |
| Blank weight | 0.606 kg |
| Machine class | L-120×400 F |
Computed for this combination. Confirm the force and the tip wall on a sample before the die is cut.
The force figure is the one people misread. 133 kN is what a single bite taking the whole 36.7 per cent reduction would need; the press in the schedule only sees 74 kN because the reduction is split. Quoting the first number for a multi-pass job is how machines get bought one size too large.
Two caveats apply throughout. First, the force figures assume a sharp, well-lapped die — a worn entry angle raises them by a fifth. Second, scrap and cycle numbers assume an operator who has run the part before, not a first-day trial.
How Carbon steel (St37 / Q235B) behaves at 36.7 per cent reduction
Mild carbon steel is the reference material for taper forming: yield around 235 MPa, elongation above 25 %, and almost no springback surprise. Most dies are proved on it before anything harder is attempted.
Carbon steel (St37 / Q235B) at this reduction behaves like a forgiving material, and the schedule above is written for that. Push the reduction per pass and the failure mode is a stretched tip that will not hold diameter, not a slow drift out of tolerance.
Typical use for this grade is lighting poles, guardrail posts, greenhouse hoops, general fabrication. If your part sits outside that list, the numbers still apply but the corrosion and fatigue assumptions behind them do not.
Medium section: 60 → 38 mm
The 60 to 38 pair is the workhorse of the trade: fork blanks, furniture legs, pole sections. Tonnage is moderate and almost every machine size can do it, so the decision usually turns on cycle time and die life.
At 60 mm the guide bushing matters as much as the die. A 60 mm tube has enough length to lever against the die entry if the bushing clearance is loose, and the symptom is ovality at the tip that looks like a die problem and is not.
Floor space and power follow the class, not the part: a L-120×400 F needs the footprint in its own datasheet whether you run 60 mm or something smaller in it.
Cost per 1,000 pieces
| Metal in the blank | 0.606 kg, 0.606 USD |
| Machine time | 12.0 s, 0.080 USD |
| Die cost, one set | 1,400 USD |
| Die life | 40,000 pieces |
| Scrap allowance | 2.2 per cent |
| Cost per piece | 0.74 USD |
| Cost per 1,000 | 737 USD |
Scrap is priced into 0.74 USD at 2.2 per cent. If your first article runs clean, the real cost is lower than this; if it does not, this number was optimistic and the difference shows up as a month of rework.
What to put on the drawing
Put the two diameters, the cone length and the wall on the drawing as basic dimensions, then tolerance the cone angle rather than the tip diameter. A tip diameter tolerance of ±0.2 mm is a different requirement at 60 mm than it is at 32 mm, and the die grinder needs to know which one you mean.
Note the grain or seam direction if the tube is welded. A longitudinal seam that lands on the die split line will open at 36.7 per cent reduction, and no amount of die polishing fixes a seam.
Send the drawing as a PDF with the dimensions readable at 100 per cent. Half the quotation delays we see come from a photo of a printout, not from a hard part.
Frequently asked questions
Can tooling be amortised across part numbers?
Only if the geometry matches. A die for a 60 to 38 cone serves any part with that geometry, so a product family shares tooling.
Is a cheap die ever right?
For a one-off prototype, yes. For anything with a repeat order, the regrind arithmetic usually kills it.
Who owns the die?
Normally the customer who paid for it. Put it in the contract, including the right to have it shipped elsewhere.
How much does the surface condition of the incoming tube matter?
More than most checklists admit. A pickled or annealed surface forms at the figures above; a scaly hot-rolled surface raises force and die wear together, and the scale is pressed into the cone where you cannot remove it.
How many can I expect in a shift?
1,968 pieces at 82 per cent utilisation, which already allows for a die check and a coil change. Add a second operator on the load side and you gain handling time only — roughly a fifth of the cycle, not half.
Talk to an engineer on WhatsApp
Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.
Chat on WhatsApp