What machining allowance after forming means at 60 → 38 mm
If you are holding a drawing with 60 → 38 mm on it and Carbon steel 20 (AISI 1020) in the material box, the machining allowance after forming call is 0.93 mm of radial stock left on the cone for the finishing cut, which is cheaper than holding the formed diameter tighter than the process can. We build that number from the reduction ratio, the wall and the yield strength, in that order, because those three move it and nothing else does.
Where the drawing calls for a thread, a face or a bore, the die has to leave stock. Too little and the thread runs out; too much and forming stops being competitive with machining.
How much stock, and where
On the outside diameter, 1.5–2 mm on diameter is the usual allowance to clean up die marks and ovality in one pass. On the tip face, 0.5–1 mm, because forming leaves the face slightly dished and not square to the axis. At this size the die sees 77 kN per bite, which is why the L-120×400 F is the natural home for the job.
On a bore, 1 mm on radius. Forming thickens the wall inward, so the bore is smaller and uneven; drilling from the formed surface without stock is how a bore ends up off-centre by 0.3 mm. Running 2 passes puts the cycle at 12.0 s and the shift output near 1,968 pieces.
The fixturing question behind the tolerance
Concentricity between the thread and the tube axis is set by how the part is held, not by how well it was formed. Chucking on the straight tube with a live centre in the cone gives the best result; chucking on the cone and hoping the jaw finds the axis does not. The tip wall finishes at 3.14 mm, 26 per cent heavier than the 2.5 mm you started with — plan the mating bore around that and not around the blank.
If concentricity is a real requirement, say it in the RFQ. It changes the process plan, the fixture and the price, and it is much cheaper to hear before the die is cut. Budget 0.77 USD per piece at this combination, of which 83 per cent is metal.
The numbers for this combination
| Tube outside diameter | 60 mm |
| Small-end diameter | 38 mm |
| Wall thickness | 2.5 mm |
| Cone length | 95 mm |
| Reduction on diameter | 36.7 per cent |
| Half angle / included angle | 6.60° / 13.2° |
| Yield strength used | 245 MPa |
| Forming force, single bite | 139 kN |
| Forming force, per bite at 2 passes | 77 kN |
| Passes | 2 passes |
| Process | cold forming |
| Cycle time | 12.0 s |
| Output per 8 h shift | 1,968 pieces |
| Tip wall after forming | 3.14 mm (+26 per cent) |
| Springback on tip diameter | 0.050 mm |
| Ovality at the tip | 1.3 per cent |
| Blank length | 171 mm |
| Blank weight | 0.606 kg |
| Machine class | L-120×400 F |
Computed for this combination. Confirm the force and the tip wall on a sample before the die is cut.
Cycle time is measured from tube-in to tube-out with the operator loading by hand. Automated loading cuts the handling element, not the forming element, so the saving is smaller than the brochure implies at this size — about a fifth of 12.0 s.
The numbers on this page are planning estimates from our own shop data for this geometry, not catalogue values. They are accurate enough to size a machine, quote a part and set a first article; they are not a substitute for a sample run in your own material.
How Carbon steel 20 (AISI 1020) behaves at 36.7 per cent reduction
A step up in carbon from St37 with the same forming behaviour. The extra 0.08 % carbon raises strength after cold work but still leaves enough ductility for a single-pass cone.
Yield strength drives the force linearly, so the jump from 235 MPa to 245 MPa is a 4 per cent heavier bite at the same geometry. Ductility drives everything else: pass count, edge condition, whether the tip cracks before the die is dialled in.
Normalise only if the part is welded afterwards or needs dimensional stability in service.
Medium section: 60 → 38 mm
The 60 to 38 pair is the workhorse of the trade: fork blanks, furniture legs, pole sections. Tonnage is moderate and almost every machine size can do it, so the decision usually turns on cycle time and die life.
Dies for this size are 40 to 60 kg: light enough to change by hand on the small end, heavy enough that a two-person lift is the safe rule at the top of the range.
If this size is a one-off rather than a family, consider buying the die and subcontracting the run. At 38,327 pieces of die life, a single order under 19,164 pieces rarely justifies the tooling on its own.
Cost per 1,000 pieces
| Metal in the blank | 0.606 kg, 0.637 USD |
| Machine time | 12.0 s, 0.080 USD |
| Die cost, one set | 1,428 USD |
| Die life | 38,327 pieces |
| Scrap allowance | 2.2 per cent |
| Cost per piece | 0.77 USD |
| Cost per 1,000 | 771 USD |
Metal is 83 per cent of the piece cost at this combination. That ratio is the reason a cheaper machine rarely changes the verdict: shaving ten per cent off the machine rate moves 0.77 USD by 0.008 USD, while shaving ten per cent off the blank moves it by more.
What to put on the drawing
Note the grain or seam direction if the tube is welded. A longitudinal seam that lands on the die split line will open at 36.7 per cent reduction, and no amount of die polishing fixes a seam.
State the material by standard and grade, not by trade name. Carbon steel 20 (AISI 1020) covers a range of yield strength wide enough to move the force by 8 kN, and the die is cut for one point in that range.
If you cannot state the cone length because the part is defined by a mating component, send the mating component instead. We will derive the cone and tell you what the resulting angle is before quoting.
Frequently asked questions
Can the die form to finished thread diameter?
Close, but the thread itself is cut or rolled. Forming to finish leaves no clean-up stock and the rolled thread inherits every die mark.
How much wall for an M36 thread on a 38 mm tip?
About 1 mm per side, so a 34 mm bore before threading. Check the actual formed section first, because the tip wall is thicker than nominal.
Does machining after forming cost much?
It is a second operation with a second setup. On high volume, forming closer to net shape and cutting only the thread is usually cheaper.
What is the first sign that the material is out of specification?
Force. A heat running 8 kN above the figure on this page has a yield strength above the certificate, and the tip will be tight before anything else moves. Check the mill certificate against the heat number before touching the die.
Can the same die run a shorter cone?
The angle is ground into the die, so a shorter cone means a smaller reduction, not the same die. You can shorten the stroke and accept a partial cone, which is sometimes acceptable for a proto and never for a production drawing.
Talk to an engineer on WhatsApp
Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.
Chat on WhatsApp