What surface finish for coating means at 152 → 114 mm
For Carbon steel 45 (AISI 1045) tube at 152 → 114 mm with a 6.0 mm wall, surface finish for coating comes down to Ra 1.2 µm on the cone flank straight out of the die, with no secondary polishing step in the routing. That single line is the answer; the rest of this page is the arithmetic behind it, so you can check the figure against your own drawing instead of taking it on trust.
A formed cone has a directional die texture. Under 60–80 microns of powder it telegraphs through, and at the tip edge the film pulls back to half thickness.
What the coater needs from the die
A fine, even texture rather than a polished mirror. Polishing looks better before coating and adheres worse after it, because there is no mechanical key. A light blast on the cone followed by phosphate is the combination that survives a salt spray test. The 2.2 per cent scrap allowance is not padding — it is the pass count and the material talking.
The tip edge needs a radius of about 0.5 mm. A sharp edge holds 15 microns where a radius holds 40, and the edge is where rust starts on every outdoor part. The mill certificate matters more than the grade name: spread inside the standard moves the force by about 61 kN.
The defects that only appear after curing
Outgassing pinholes come from air or moisture trapped in a lap or a porous weld, expanding at curing temperature. The fix is upstream: find the lap and stop making it. At this size the die sees 566 kN per bite, which is why the L-160×600 CNC is the natural home for the job.
Edge pull-back is a coverage problem, not an adhesion problem, and adding a second coat does not fix it because the second coat pulls back too. Running 2 passes puts the cycle at 17.9 s and the shift output near 1,319 pieces.
The numbers for this combination
| Tube outside diameter | 152 mm |
| Small-end diameter | 114 mm |
| Wall thickness | 6.0 mm |
| Cone length | 250 mm |
| Reduction on diameter | 25.0 per cent |
| Half angle / included angle | 4.35° / 8.7° |
| Yield strength used | 355 MPa |
| Forming force, single bite | 1,020 kN |
| Forming force, per bite at 2 passes | 566 kN |
| Passes | 2 passes |
| Process | cold forming |
| Cycle time | 17.9 s |
| Output per 8 h shift | 1,319 pieces |
| Tip wall after forming | 6.93 mm (+15 per cent) |
| Springback on tip diameter | 0.23 mm |
| Ovality at the tip | 0.8 per cent |
| Blank length | 427 mm |
| Blank weight | 9.22 kg |
| Machine class | L-160×600 CNC |
Computed for this combination. Confirm the force and the tip wall on a sample before the die is cut.
The blank length assumes you grip 167 mm of straight tube in the collet and trim 10 mm after forming. If your chuck is longer, add it to 427 mm — the cone itself does not change, only the material you pay for.
Where a number depends on the heat of steel rather than on the geometry, it is flagged. Those are the figures to re-measure on the first batch instead of copying from this page.
How Carbon steel 45 (AISI 1045) behaves at 25.0 per cent reduction
Medium carbon: noticeably stronger, noticeably less forgiving. Springback is 30–40 % higher than mild steel, and the tip crack window narrows because the material has less elongation left before the die touches it.
In practice the first thing to change with Carbon steel 45 (AISI 1045) is not the die but the lubricant film. steel 45 will form on a marginal film for a hundred pieces and then start picking up on the die — the mark appears long before the dimension moves.
At 25.0 per cent reduction the work-hardening from forming is worth roughly 78 MPa of extra yield at the tip. If your next operation is machining, that is helpful; if it is another forming pass, budget for it.
Extra-large section: 152 → 114 mm
Extra-large cones are almost always hot formed or formed in two stages. The wall is thick enough that cold flow becomes unpredictable and the die sees loads that shorten its life fast.
The 427 mm blank is heavy enough — 9.22 kg — that manual loading sets the pace before the forming stroke does. That is why the cycle sits at 17.9 s rather than the 14.0 s the stroke alone would allow.
Machine class for 152 mm is the L-160×600 CNC. Going one class up buys stiffness you will not use at this diameter and costs floor space you will miss.
Cost per 1,000 pieces
| Metal in the blank | 9.22 kg, 10.147 USD |
| Machine time | 17.9 s, 0.273 USD |
| Die cost, one set | 6,844 USD |
| Die life | 4,851 pieces |
| Scrap allowance | 2.2 per cent |
| Cost per piece | 12.10 USD |
| Cost per 1,000 | 12,098 USD |
The 12.10 USD figure excludes finishing, coating and packing. It is the formed part at the machine, which is the only number that lets you compare two processes fairly.
What to put on the drawing
Add the as-formed wall at the tip as a reference dimension with a minimum. It is the dimension that decides whether the mating bore cleans up, and it is the one most often left off.
Put the two diameters, the cone length and the wall on the drawing as basic dimensions, then tolerance the cone angle rather than the tip diameter. A tip diameter tolerance of ±0.2 mm is a different requirement at 152 mm than it is at 32 mm, and the die grinder needs to know which one you mean.
If you cannot state the cone length because the part is defined by a mating component, send the mating component instead. We will derive the cone and tell you what the resulting angle is before quoting.
Frequently asked questions
Can a formed cone be galvanized?
Yes, with drain holes and a wall thick enough not to distort at 450 °C. Thin-wall cones warp.
Does the die texture affect coating cost?
Indirectly: a rough cone needs more pretreatment and sometimes a primer, which is a per-part cost forever.
What surface roughness should I specify?
Ra 1.6–3.2 on the cone is a practical range for powder. Finer is not better without a blast.
Does the heat treatment number change with wall thickness?
Yes — soak time scales with section, not with the part. 600 °C is right for this grade, but a 6.0 mm wall needs the 1 h per 25 mm of section at temperature, not the twenty-minute cycle that works on thin sheet.
What tube tolerance should I buy?
±0.15 mm on outside diameter and ±10 per cent on wall for this geometry. Tighter than that costs money at the mill and buys you nothing the die cannot absorb; looser than that and the 0.8 per cent ovality figure stops holding.
Talk to an engineer on WhatsApp
Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.
Chat on WhatsApp