What cut quality before forming means at 114 → 76 mm
If you are holding a drawing with 114 → 76 mm on it and Stainless 316L (03Kh17N14M2) in the material box, the cut quality before forming call is a cut held to ±0.8 mm with burr under 0.20 mm, because a burr that survives forming becomes a crack initiation site at the tip. We build that number from the reduction ratio, the wall and the yield strength, in that order, because those three move it and nothing else does.
The die meets the tube edge before anything else. A square, burr-free cut is the cheapest quality improvement in the whole line, and a bad one mimics every die fault there is.
The two numbers that matter
Squareness within 0.5 mm across the diameter, and burr under 0.2 mm on the inside. A slanted face makes the die contact a line rather than a ring: the high side takes all the load first, the cone comes out oval, and the operator blames the die. The tip wall finishes at 6.12 mm, 22 per cent heavier than the 5.0 mm you started with — plan the mating bore around that and not around the blank.
An internal burr is worse because it is invisible. It gets rolled into the cone wall, leaves a fold line, and on a fatigue part becomes the crack origin. You cannot inspect it from outside after forming. Budget 17.80 USD per piece at this combination, of which 92 per cent is metal.
What to change, and in what order
Clamp pressure first — a loose clamp on a cold saw produces a slanted cut with a perfect blade. Then blade condition, then feed rate. On a CNC tube cutter, the chamfer head removes the burr in the same cycle and is usually cheaper than a separate deburr station. Springback adds 0.11 mm to the tip diameter, so the die is cut that much under nominal.
Abrasive saws cut fast and leave a heat-affected edge and a heavy burr. They are acceptable for structural parts and unacceptable for anything that will be tapered and then loaded. 8,346 pieces per die set is the working number here; below 4,173 pieces a year the tooling never pays back.
The numbers for this combination
| Tube outside diameter | 114 mm |
| Small-end diameter | 76 mm |
| Wall thickness | 5.0 mm |
| Cone length | 190 mm |
| Reduction on diameter | 33.3 per cent |
| Half angle / included angle | 5.71° / 11.4° |
| Yield strength used | 205 MPa |
| Forming force, single bite | 421 kN |
| Forming force, per bite at 3 passes | 165 kN |
| Passes | 3 passes |
| Process | cold forming |
| Cycle time | 19.1 s |
| Output per 8 h shift | 1,236 pieces |
| Tip wall after forming | 6.12 mm (+22 per cent) |
| Springback on tip diameter | 0.11 mm |
| Ovality at the tip | 0.9 per cent |
| Blank length | 325 mm |
| Blank weight | 4.41 kg |
| Machine class | L-120×400 F |
Computed for this combination. Confirm the force and the tip wall on a sample before the die is cut.
The blank length assumes you grip 125 mm of straight tube in the collet and trim 10 mm after forming. If your chuck is longer, add it to 325 mm — the cone itself does not change, only the material you pay for.
The numbers on this page are planning estimates from our own shop data for this geometry, not catalogue values. They are accurate enough to size a machine, quote a part and set a first article; they are not a substitute for a sample run in your own material.
How Stainless 316L (03Kh17N14M2) behaves at 33.3 per cent reduction
Softer than 304 at the start and just as eager to work-harden. Molybdenum makes it galling-prone in a different way: it welds to the die rather than scratching it.
Yield strength drives the force linearly, so the jump from 235 MPa to 205 MPa is a -13 per cent heavier bite at the same geometry. Ductility drives everything else: pass count, edge condition, whether the tip cracks before the die is dialled in.
At 33.3 per cent reduction the work-hardening from forming is worth roughly 45 MPa of extra yield at the tip. If your next operation is machining, that is helpful; if it is another forming pass, budget for it.
Heavy section: 114 → 76 mm
Heavy sections are where hot forming enters the conversation. Cold is still possible on mild steel, but the machine is 200 tonnes class and the tooling cost is not a rounding error.
Dies for this size are 40 to 60 kg: light enough to change by hand on the small end, heavy enough that a two-person lift is the safe rule at the top of the range.
Machine class for 114 mm is the L-120×400 F. Going one class up buys stiffness you will not use at this diameter and costs floor space you will miss.
Cost per 1,000 pieces
| Metal in the blank | 4.41 kg, 16.327 USD |
| Machine time | 19.1 s, 0.223 USD |
| Die cost, one set | 6,156 USD |
| Die life | 8,346 pieces |
| Scrap allowance | 2.9 per cent |
| Cost per piece | 17.80 USD |
| Cost per 1,000 | 17,804 USD |
The 17.80 USD figure excludes finishing, coating and packing. It is the formed part at the machine, which is the only number that lets you compare two processes fairly.
What to put on the drawing
Note the grain or seam direction if the tube is welded. A longitudinal seam that lands on the die split line will open at 33.3 per cent reduction, and no amount of die polishing fixes a seam.
State the material by standard and grade, not by trade name. Stainless 316L (03Kh17N14M2) covers a range of yield strength wide enough to move the force by 25 kN, and the die is cut for one point in that range.
If you cannot state the cone length because the part is defined by a mating component, send the mating component instead. We will derive the cone and tell you what the resulting angle is before quoting.
Frequently asked questions
Does cut quality matter on thick wall?
Less for cracking, more for squareness. A thick wall forgives the burr and punishes the angle.
Can I inspect burr without pulling parts?
A mirror and a torch at the machine, ten parts an hour. Cheaper than the scrap it prevents.
Does the cut affect cycle time?
Only through rework. A part that needs deburring adds 5–15 seconds that never appear in the cycle-time quote.
What is the first sign that the material is out of specification?
Force. A heat running 25 kN above the figure on this page has a yield strength above the certificate, and the tip will be tight before anything else moves. Check the mill certificate against the heat number before touching the die.
Can the same die run a shorter cone?
The angle is ground into the die, so a shorter cone means a smaller reduction, not the same die. You can shorten the stroke and accept a partial cone, which is sometimes acceptable for a proto and never for a production drawing.