What heat treatment after forming means at 76 → 48 mm
Short version for Stainless 316L (03Kh17N14M2) at 76 → 48 mm: 400 °C for 1 h, furnace cool after forming, air cooled, which removes the formed-in stress without touching the hardness. It is worth knowing why before you accept it, because the same three inputs that produce this answer will produce a different one the moment the wall or the grade changes.
Forming leaves the cone work-hardened and stressed. Whether that matters depends on what the part does next: nothing, machining, welding, or cyclic loading.
Three levels of treatment
Stress relief at 550–650 °C for one hour per 25 mm of section removes residual stress and leaves the strength roughly where it was. That is enough for parts that will be machined or coated and not loaded heavily. Running 2 passes puts the cycle at 13.6 s and the shift output near 1,736 pieces.
Normalising refines the structure and restores ductility, at the cost of the cold-work strength. Full anneal is for parts that will be formed again or machined extensively. The tip wall finishes at 4.40 mm, 26 per cent heavier than the 3.5 mm you started with — plan the mating bore around that and not around the blank.
When you can skip it
On mild steel with a moderate reduction and no fatigue duty, nothing is needed. On 4130, 4140, 45 or any stainless that will be welded, skipping it is how the weld cracks three weeks later. Budget 5.44 USD per piece at this combination, of which 92 per cent is metal.
The honest test: if the drawing shows a fatigue life, a weld, or a thread at the tip, treat it. If it shows a decorative cone, do not. Springback adds 0.072 mm to the tip diameter, so the die is cut that much under nominal.
The numbers for this combination
| Tube outside diameter | 76 mm |
| Small-end diameter | 48 mm |
| Wall thickness | 3.5 mm |
| Cone length | 120 mm |
| Reduction on diameter | 36.8 per cent |
| Half angle / included angle | 6.65° / 13.3° |
| Yield strength used | 205 MPa |
| Forming force, single bite | 207 kN |
| Forming force, per bite at 2 passes | 115 kN |
| Passes | 2 passes |
| Process | cold forming |
| Cycle time | 13.6 s |
| Output per 8 h shift | 1,736 pieces |
| Tip wall after forming | 4.40 mm (+26 per cent) |
| Springback on tip diameter | 0.072 mm |
| Ovality at the tip | 1.2 per cent |
| Blank length | 214 mm |
| Blank weight | 1.35 kg |
| Machine class | L-120×400 F |
Computed for this combination. Confirm the force and the tip wall on a sample before the die is cut.
Wall thickening is not optional and it is not uniform. 4.40 mm at the tip is the thin-wall constant-volume answer; on a real part expect the last few millimetres of cone to run a little heavier because the material has nowhere to go.
Two caveats apply throughout. First, the force figures assume a sharp, well-lapped die — a worn entry angle raises them by a fifth. Second, scrap and cycle numbers assume an operator who has run the part before, not a first-day trial.
How Stainless 316L (03Kh17N14M2) behaves at 36.8 per cent reduction
Softer than 304 at the start and just as eager to work-harden. Molybdenum makes it galling-prone in a different way: it welds to the die rather than scratching it.
Stainless 316L (03Kh17N14M2) at this reduction behaves like a workable material, and the schedule above is written for that. Push the reduction per pass and the failure mode is a roughened cone that needs polishing, not a slow drift out of tolerance.
Do not skip that step on a fatigue part. A formed cone carries residual stress that is invisible on the drawing and obvious on a bend test after six months in service.
Large section: 76 → 48 mm
At 76 mm the force starts to matter: the same wall needs roughly twice the tonnage of a 60 mm part, and the guide bushing has to control a heavier tube.
At 76 mm the guide bushing matters as much as the die. A 76 mm tube has enough length to lever against the die entry if the bushing clearance is loose, and the symptom is ovality at the tip that looks like a die problem and is not.
The next size up shares the same machine but not the same die, and the changeover is 50 minutes. Plan families of parts around that number rather than around the cycle time.
Cost per 1,000 pieces
| Metal in the blank | 1.35 kg, 5.005 USD |
| Machine time | 13.6 s, 0.113 USD |
| Die cost, one set | 3,564 USD |
| Die life | 17,387 pieces |
| Scrap allowance | 2.2 per cent |
| Cost per piece | 5.44 USD |
| Cost per 1,000 | 5,444 USD |
Die cost is 0.205 USD per piece here — small enough to ignore on a long run and large enough to matter on a short one. The break-even is around 8189 pieces.
What to put on the drawing
Put the two diameters, the cone length and the wall on the drawing as basic dimensions, then tolerance the cone angle rather than the tip diameter. A tip diameter tolerance of ±0.2 mm is a different requirement at 76 mm than it is at 32 mm, and the die grinder needs to know which one you mean.
Note the grain or seam direction if the tube is welded. A longitudinal seam that lands on the die split line will open at 36.8 per cent reduction, and no amount of die polishing fixes a seam.
Send the drawing as a PDF with the dimensions readable at 100 per cent. Half the quotation delays we see come from a photo of a printout, not from a hard part.
Frequently asked questions
Does heat treatment change the cone dimensions?
Yes, by 0.05–0.15 mm on diameter through stress relaxation. Size-critical parts are finished after treatment, not before.
Can I stress relieve in a furnace with the parts stacked?
Only if the stack is open enough to heat evenly. A tight bundle heats unevenly and leaves one end stressed, which is worse than doing nothing.
Is induction heating enough?
For local stress relief on a small zone, yes. For whole-part normalising, no.
How much does the surface condition of the incoming tube matter?
More than most checklists admit. A pickled or annealed surface forms at the figures above; a scaly hot-rolled surface raises force and die wear together, and the scale is pressed into the cone where you cannot remove it.
How many can I expect in a shift?
1,736 pieces at 82 per cent utilisation, which already allows for a die check and a coil change. Add a second operator on the load side and you gain handling time only — roughly a fifth of the cycle, not half.
Talk to an engineer on WhatsApp
Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.
Chat on WhatsApp