What springback compensation means at 32 → 20 mm

If you are holding a drawing with 32 → 20 mm on it and Stainless 316L (03Kh17N14M2) in the material box, the springback compensation call is 0.030 mm of springback on the tip diameter, cut into the die instead of being chased with a second operation. We build that number from the reduction ratio, the wall and the yield strength, in that order, because those three move it and nothing else does.

Every cone springs back when the die releases. The size you cut into the die is not the size that comes out, and the difference is predictable once you measure the first article.

How much, and in which direction

Springback shows up as an oversize tip: the part comes out 0.1–0.4 % larger than the die, more on high-yield material, more on large diameters, and much more on aluminium. A 38 mm tip on 4130 can come out 0.12 mm over; the same tip on 6061-T6 can be 0.25 mm over. The tip wall finishes at 1.90 mm, 26 per cent heavier than the 1.5 mm you started with — plan the mating bore around that and not around the blank.

The compensation is to cut the die undersize by the measured amount and then re-check on the second article. Guessing from a table is how a die gets scrapped: the table gives a starting point, the first article gives the number. Budget 0.51 USD per piece at this combination, of which 82 per cent is metal.

Why the second article matters more than the first

The first part off a fresh die often runs small because the die has not yet been polished by the material. By part three or four the size stabilises. Sizing the die from part one leads to an oversize die and a permanent offset. Springback adds 0.030 mm to the tip diameter, so the die is cut that much under nominal.

So the procedure is: form five, measure all five, discard the first, and set the die from the median of the last four. That single habit removes most of the size drift between batches. 41,729 pieces per die set is the working number here; below 20,865 pieces a year the tooling never pays back.

The numbers for this combination

Tube outside diameter32 mm
Small-end diameter20 mm
Wall thickness1.5 mm
Cone length55 mm
Reduction on diameter37.5 per cent
Half angle / included angle6.23° / 12.5°
Yield strength used205 MPa
Forming force, single bite38 kN
Forming force, per bite at 2 passes21 kN
Passes2 passes
Processcold forming
Cycle time8.8 s
Output per 8 h shift2,683 pieces
Tip wall after forming1.90 mm (+26 per cent)
Springback on tip diameter0.030 mm
Ovality at the tip1.6 per cent
Blank length100 mm
Blank weight0.114 kg
Machine classØ50 class (manual or automatic)

Computed for this combination. Confirm the force and the tip wall on a sample before the die is cut.

The blank length assumes you grip 35 mm of straight tube in the collet and trim 10 mm after forming. If your chuck is longer, add it to 100 mm — the cone itself does not change, only the material you pay for.

Two caveats apply throughout. First, the force figures assume a sharp, well-lapped die — a worn entry angle raises them by a fifth. Second, scrap and cycle numbers assume an operator who has run the part before, not a first-day trial.

How Stainless 316L (03Kh17N14M2) behaves at 37.5 per cent reduction

Softer than 304 at the start and just as eager to work-harden. Molybdenum makes it galling-prone in a different way: it welds to the die rather than scratching it.

Yield strength drives the force linearly, so the jump from 235 MPa to 205 MPa is a -13 per cent heavier bite at the same geometry. Ductility drives everything else: pass count, edge condition, whether the tip cracks before the die is dialled in.

At 37.5 per cent reduction the work-hardening from forming is worth roughly 45 MPa of extra yield at the tip. If your next operation is machining, that is helpful; if it is another forming pass, budget for it.

Small section: 32 → 20 mm

Small sections are dominated by handling, not by force. The die is light, the cycle is short, and the biggest quality risk is ovality from manual loading rather than tonnage.

Dies for this size are under 20 kg: light enough to change by hand on the small end, heavy enough that a two-person lift is the safe rule at the top of the range.

Machine class for 32 mm is the Ø50 class (manual or automatic). Going one class up buys stiffness you will not use at this diameter and costs floor space you will miss.

Cost per 1,000 pieces

Metal in the blank0.114 kg, 0.422 USD
Machine time8.8 s, 0.044 USD
Die cost, one set1,458 USD
Die life41,729 pieces
Scrap allowance2.2 per cent
Cost per piece0.51 USD
Cost per 1,000512 USD

The 0.51 USD figure excludes finishing, coating and packing. It is the formed part at the machine, which is the only number that lets you compare two processes fairly.

What to put on the drawing

Put the two diameters, the cone length and the wall on the drawing as basic dimensions, then tolerance the cone angle rather than the tip diameter. A tip diameter tolerance of ±0.2 mm is a different requirement at 32 mm than it is at 32 mm, and the die grinder needs to know which one you mean.

Note the grain or seam direction if the tube is welded. A longitudinal seam that lands on the die split line will open at 37.5 per cent reduction, and no amount of die polishing fixes a seam.

If you cannot state the cone length because the part is defined by a mating component, send the mating component instead. We will derive the cone and tell you what the resulting angle is before quoting.

Frequently asked questions

Can springback be removed by dwell?

Dwell helps by letting the material creep under load, typically recovering 20–30 % of the springback. It does not remove it, and long dwell costs cycle time on every part.

Does lubrication change springback?

Indirectly, by changing friction and therefore the stress state. A change of lubricant can move the tip size by 0.05 mm, which is enough to matter on a tolerance of ±0.15 mm.

How do I compensate on a die that is already made?

Polish the tip land or adjust the stroke to move the cone, and if the size is still out, the die has to be re-cut. This is why the first article protocol exists.

How much does the surface condition of the incoming tube matter?

More than most checklists admit. A pickled or annealed surface forms at the figures above; a scaly hot-rolled surface raises force and die wear together, and the scale is pressed into the cone where you cannot remove it.

How many can I expect in a shift?

2,683 pieces at 82 per cent utilisation, which already allows for a die check and a coil change. Add a second operator on the load side and you gain handling time only — roughly a fifth of the cycle, not half.

Talk to an engineer on WhatsApp

Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.

Chat on WhatsApp