What a 100 → 62 mm taper asks of the die
This geometry removes 38.0 per cent from the outside diameter over a 250 mm cone. The included cone angle is 8.7°, and at a 4.0 mm starting wall the material has to flow inward rather than be cut away.
Force is driven by the 235 MPa yield, the 4.0 mm wall and the 38.0 per cent reduction. One bite means 362 kN; with 2 passes the die sees around 201 kN.
Tip wall and springback on this part
Constant volume puts the wall at the small end near 5.08 mm, 27 per cent heavier than the 4.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.
Measure the cold part: recovery on this grade is about 0.077 mm on diameter and ovality near 1.2 per cent. Ring-gauge at a fixed distance from the end every time.
How carbon steel behaves at 100 mm outside diameter
Mild carbon steel is the reference material for taper forming: yield around 235 MPa, elongation above 25 %, and almost no springback surprise. Most dies are proved on it before anything harder is attempted.
The first article is the only moment when both sides can disagree cheaply. A protocol with five parts and six numbers prevents most of the arguments that follow a shipment.
At 235 MPa yield with high ductility, this grade needs 2 passes on this geometry. The die is expected to last 7,000 pieces before the first re-polish, and the stress-relief practice is: No heat treatment needed unless the part is fatigue-loaded; a 550–600 °C stress relief removes the formed-in stress.
Typical applications are lighting poles, guardrail posts, greenhouse hoops, general fabrication. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.
Cycle, tooling and piece cost
Cycle time is about 17.9 seconds from tube in to tube out, which is roughly 1,319 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 7,000 pieces before the first re-polish.
At the current price band the formed part costs about 4.71 USD, of which roughly 74 per cent is the blank. The recommended class is the L-120×400 F; a larger frame buys stiffness this diameter does not use.
How to quote this geometry
A readable drawing with OD, tip, cone length, wall and grade is enough for a first quote. Add the downstream operation so the allowance and the stress relief are specified rather than assumed.
For Carbon steel (St37 / Q235B) the decision that moves the number most is first article approval. Say what you need there before asking for a price.
Frequently asked questions
What machine class forms a 100 → 62 mm tube?
The L-120×400 F. Forming force is about 201 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.
How much thicker is the tip?
From 4.0 mm to about 5.08 mm, an increase of 27 per cent. Machine the bore after forming if the fit is tight.
What should I put on the drawing?
The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.077 mm on the die.
Talk to an engineer on WhatsApp
Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.
Chat on WhatsApp