What a 100 → 62 mm taper asks of the die
This geometry removes 37.5 per cent from the outside diameter over a 250 mm cone. The included cone angle is 8.6°, and at a 1.5 mm starting wall the material has to flow inward rather than be cut away.
If this cone were formed in one stroke the die would take 141 kN. Our schedule uses 2 passes, bringing the per-bite load to 78 kN and leaving margin on the frame.
Tip wall and springback on this part
Constant volume puts the wall at the small end near 1.90 mm, 26 per cent heavier than the 1.5 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.
Elastic recovery adds about 0.067 mm to the tip diameter and typical ovality is 1.6 per cent. Compensate the recovery in the die rather than with the machine stop.
How steel 20 behaves at 100 mm outside diameter
A step up in carbon from St37 with the same forming behaviour. The extra 0.08 % carbon raises strength after cold work but still leaves enough ductility for a single-pass cone.
A cycle time is a promise about capacity. Quoting the fastest stroke instead of the average cycle is how a shift plan fails in the second week.
At 245 MPa yield with high ductility, this grade needs 2 passes on this geometry. The die is expected to last 6,707 pieces before the first re-polish, and the stress-relief practice is: Normalise only if the part is welded afterwards or needs dimensional stability in service.
Typical applications are shafts, bushes, fork blanks, ground screw tips. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.
Cycle, tooling and piece cost
Cycle time is about 17.9 seconds from tube in to tube out, which is roughly 1,319 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 6,707 pieces before the first re-polish.
Budget 2.63 USD per formed piece. Metal accounts for about 54 per cent of that, so the L-120×400 F is the sensible class rather than the next size up.
How to quote this geometry
If your part sits between two standard families, this page is the exact version and the case library is the decision matrix. Send either one with your quantity.
For Carbon steel 20 (AISI 1020) the decision that moves the number most is cycle time planning. Say what you need there before asking for a price.
Frequently asked questions
What machine class forms a 100 → 62 mm tube?
The L-120×400 F. Forming force is about 78 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.
How much thicker is the tip?
From 1.5 mm to about 1.90 mm, an increase of 26 per cent. Machine the bore after forming if the fit is tight.
What should I put on the drawing?
The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.067 mm on the die.
Talk to an engineer on WhatsApp
Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.
Chat on WhatsApp