What a 32 → 20 mm taper asks of the die

This geometry removes 37.5 per cent from the outside diameter over a 95 mm cone. The included cone angle is 7.2°, and at a 1.0 mm starting wall the material has to flow inward rather than be cut away.

If this cone were formed in one stroke the die would take 43 kN. Our schedule uses 2 passes, bringing the per-bite load to 24 kN and leaving margin on the frame.

Tip wall and springback on this part

Constant volume puts the wall at the small end near 1.26 mm, 26 per cent heavier than the 1.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.

Elastic recovery adds about 0.041 mm to the tip diameter and typical ovality is 2.0 per cent. Compensate the recovery in the die rather than with the machine stop.

How steel 45 behaves at 32 mm outside diameter

Medium carbon: noticeably stronger, noticeably less forgiving. Springback is 30–40 % higher than mild steel, and the tip crack window narrows because the material has less elongation left before the die touches it.

Where the drawing calls for a thread, a face or a bore, the die has to leave stock. Too little and the thread runs out; too much and forming stops being competitive with machining.

At 355 MPa yield with medium ductility, this grade needs 2 passes on this geometry. The die is expected to last 27,722 pieces before the first re-polish, and the stress-relief practice is: Normalise after forming whenever the part sees bending or cyclic load.

Typical applications are shafts, spindles, load-bearing pins. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.

Cycle, tooling and piece cost

Cycle time is about 9.9 seconds from tube in to tube out, which is roughly 2,385 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 27,722 pieces before the first re-polish.

Budget 0.25 USD per formed piece. Metal accounts for about 47 per cent of that, so the Ø50 class (manual or automatic) is the sensible class rather than the next size up.

How to quote this geometry

If your part sits between two standard families, this page is the exact version and the case library is the decision matrix. Send either one with your quantity.

For Carbon steel 45 (AISI 1045) the decision that moves the number most is machining allowance after forming. Say what you need there before asking for a price.

Frequently asked questions

What machine class forms a 32 → 20 mm tube?

The Ø50 class (manual or automatic). Forming force is about 24 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.

How much thicker is the tip?

From 1.0 mm to about 1.26 mm, an increase of 26 per cent. Machine the bore after forming if the fit is tight.

What should I put on the drawing?

The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.041 mm on the die.

Talk to an engineer on WhatsApp

Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.

Chat on WhatsApp