What a 35 → 22 mm taper asks of the die
This geometry removes 37.4 per cent from the outside diameter over a 95 mm cone. The included cone angle is 7.9°, and at a 1.0 mm starting wall the material has to flow inward rather than be cut away.
The raw estimate is 27 kN for one bite. Split into 2 passes it becomes about 15 kN per bite, and the difference is the whole reason to plan the passes before choosing a press.
Tip wall and springback on this part
Constant volume puts the wall at the small end near 1.26 mm, 26 per cent heavier than the 1.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.
The tip comes back 0.029 mm larger than the die once the load is released. Ovality around 2.0 per cent is normal and is held down by a full-length guide bushing.
How 316L stainless behaves at 35 mm outside diameter
Softer than 304 at the start and just as eager to work-harden. Molybdenum makes it galling-prone in a different way: it welds to the die rather than scratching it.
Die life is quoted in parts, not months. If a supplier answers "about a year", they have not measured it, and the number you plan capacity on is a guess.
At 205 MPa yield with medium ductility, this grade needs 2 passes on this geometry. The die is expected to last 27,820 pieces before the first re-polish, and the stress-relief practice is: Anneal after heavy deformation; low carbon means no sensitisation risk at the weld.
Typical applications are chemical plant, marine hardware, medical frames. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.
Cycle, tooling and piece cost
Cycle time is about 10.2 seconds from tube in to tube out, which is roughly 2,315 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 27,820 pieces before the first re-polish.
Raw material is 73 per cent of the 0.61 USD piece cost here. That ratio is why the Ø50 class (manual or automatic) and not a heavier frame is the economic choice at this diameter.
How to quote this geometry
Send the two diameters, the cone length, the wall and the grade. State what you need on die life and regrind interval before asking for a price, because that decision drives the tooling.
For Stainless 316L (03Kh17N14M2) the decision that moves the number most is die life and regrind interval. Say what you need there before asking for a price.
Frequently asked questions
What machine class forms a 35 → 22 mm tube?
The Ø50 class (manual or automatic). Forming force is about 15 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.
How much thicker is the tip?
From 1.0 mm to about 1.26 mm, an increase of 26 per cent. Machine the bore after forming if the fit is tight.
What should I put on the drawing?
The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.029 mm on the die.
Talk to an engineer on WhatsApp
Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.
Chat on WhatsApp