What a 35 → 22 mm taper asks of the die

This geometry removes 37.4 per cent from the outside diameter over a 95 mm cone. The included cone angle is 7.9°, and at a 4.0 mm starting wall the material has to flow inward rather than be cut away.

Force is driven by the 275 MPa yield, the 4.0 mm wall and the 37.4 per cent reduction. One bite means 147 kN; with 3 passes the die sees around 58 kN.

Tip wall and springback on this part

Constant volume puts the wall at the small end near 5.21 mm, 30 per cent heavier than the 4.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.

Measure the cold part: recovery on this grade is about 0.047 mm on diameter and ovality near 1.4 per cent. Ring-gauge at a fixed distance from the end every time.

How 6061-T6 behaves at 35 mm outside diameter

Forms at a third of the tonnage of steel and springs back three times as much. T6 temper is already precipitation-hardened, so the cone can crack if the reduction is aggressive.

A wrinkle is a stability failure: the wall buckles in compression before it can thicken. Adding force makes it worse, which is why every instinct at the machine is wrong here.

At 275 MPa yield with low ductility, this grade needs 3 passes on this geometry. The die is expected to last 32,756 pieces before the first re-polish, and the stress-relief practice is: Form in T4 and age to T6 afterwards where the drawing allows; T6 stock limits reduction per pass.

Typical applications are handlebars, seatposts, tent poles, display frames. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.

Cycle, tooling and piece cost

Cycle time is about 12.7 seconds from tube in to tube out, which is roughly 1,859 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 32,756 pieces before the first re-polish.

At the current price band the formed part costs about 0.49 USD, of which roughly 67 per cent is the blank. The recommended class is the Ø50 class (manual or automatic); a larger frame buys stiffness this diameter does not use.

How to quote this geometry

A readable drawing with OD, tip, cone length, wall and grade is enough for a first quote. Add the downstream operation so the allowance and the stress relief are specified rather than assumed.

For Aluminium 6061-T6 the decision that moves the number most is wrinkling on thin wall. Say what you need there before asking for a price.

Frequently asked questions

What machine class forms a 35 → 22 mm tube?

The Ø50 class (manual or automatic). Forming force is about 58 kN per bite with 3 passes, so a smaller frame will deflect before it stalls.

How much thicker is the tip?

From 4.0 mm to about 5.21 mm, an increase of 30 per cent. Machine the bore after forming if the fit is tight.

What should I put on the drawing?

The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.047 mm on the die.

Talk to an engineer on WhatsApp

Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.

Chat on WhatsApp