What a 42 → 25 mm taper asks of the die
This geometry removes 40.5 per cent from the outside diameter over a 120 mm cone. The included cone angle is 8.1°, and at a 2.0 mm starting wall the material has to flow inward rather than be cut away.
If this cone were formed in one stroke the die would take 92 kN. Our schedule uses 3 passes, bringing the per-bite load to 36 kN and leaving margin on the frame.
Tip wall and springback on this part
Constant volume puts the wall at the small end near 2.67 mm, 34 per cent heavier than the 2.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.
Elastic recovery adds about 0.038 mm to the tip diameter and typical ovality is 1.8 per cent. Compensate the recovery in the die rather than with the machine stop.
How 6061-T6 behaves at 42 mm outside diameter
Forms at a third of the tonnage of steel and springs back three times as much. T6 temper is already precipitation-hardened, so the cone can crack if the reduction is aggressive.
Inspection on a tapered part fails when it is done at the wrong moment with the wrong tool. A plan is three decisions: what, how often, and with what.
At 275 MPa yield with low ductility, this grade needs 3 passes on this geometry. The die is expected to last 20,473 pieces before the first re-polish, and the stress-relief practice is: Form in T4 and age to T6 afterwards where the drawing allows; T6 stock limits reduction per pass.
Typical applications are handlebars, seatposts, tent poles, display frames. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.
Cycle, tooling and piece cost
Cycle time is about 14.4 seconds from tube in to tube out, which is roughly 1,640 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 20,473 pieces before the first re-polish.
Budget 0.55 USD per formed piece. Metal accounts for about 48 per cent of that, so the Ø50 class (manual or automatic) is the sensible class rather than the next size up.
How to quote this geometry
If your part sits between two standard families, this page is the exact version and the case library is the decision matrix. Send either one with your quantity.
For Aluminium 6061-T6 the decision that moves the number most is dimensional inspection plan. Say what you need there before asking for a price.
Frequently asked questions
What machine class forms a 42 → 25 mm tube?
The Ø50 class (manual or automatic). Forming force is about 36 kN per bite with 3 passes, so a smaller frame will deflect before it stalls.
How much thicker is the tip?
From 2.0 mm to about 2.67 mm, an increase of 34 per cent. Machine the bore after forming if the fit is tight.
What should I put on the drawing?
The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.038 mm on the die.