What a 42 → 25 mm taper asks of the die

This geometry removes 40.5 per cent from the outside diameter over a 120 mm cone. The included cone angle is 8.1°, and at a 2.0 mm starting wall the material has to flow inward rather than be cut away.

The raw estimate is 72 kN for one bite. Split into 2 passes it becomes about 40 kN per bite, and the difference is the whole reason to plan the passes before choosing a press.

Tip wall and springback on this part

Constant volume puts the wall at the small end near 2.59 mm, 30 per cent heavier than the 2.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.

The tip comes back 0.040 mm larger than the die once the load is released. Ovality around 1.5 per cent is normal and is held down by a full-length guide bushing.

How 304 stainless behaves at 42 mm outside diameter

Low yield but severe work hardening: the cone gets hard as it forms, so the die load climbs through the stroke. Galling is the main risk and it is a lubrication problem before it is a die problem.

Where the drawing calls for a thread, a face or a bore, the die has to leave stock. Too little and the thread runs out; too much and forming stops being competitive with machining.

At 215 MPa yield with medium ductility, this grade needs 2 passes on this geometry. The die is expected to last 17,502 pieces before the first re-polish, and the stress-relief practice is: Solution anneal if deformation exceeds about 15 %, otherwise corrosion resistance in the cone drops.

Typical applications are food equipment, architectural tube, exhaust tips. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.

Cycle, tooling and piece cost

Cycle time is about 11.7 seconds from tube in to tube out, which is roughly 2,018 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 17,502 pieces before the first re-polish.

Raw material is 78 per cent of the 1.45 USD piece cost here. That ratio is why the Ø50 class (manual or automatic) and not a heavier frame is the economic choice at this diameter.

How to quote this geometry

Send the two diameters, the cone length, the wall and the grade. State what you need on machining allowance after forming before asking for a price, because that decision drives the tooling.

For Stainless 304 (08Kh18N10) the decision that moves the number most is machining allowance after forming. Say what you need there before asking for a price.

Frequently asked questions

What machine class forms a 42 → 25 mm tube?

The Ø50 class (manual or automatic). Forming force is about 40 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.

How much thicker is the tip?

From 2.0 mm to about 2.59 mm, an increase of 30 per cent. Machine the bore after forming if the fit is tight.

What should I put on the drawing?

The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.040 mm on the die.

Talk to an engineer on WhatsApp

Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.

Chat on WhatsApp