What a 50 → 31 mm taper asks of the die
This geometry removes 37.6 per cent from the outside diameter over a 120 mm cone. The included cone angle is 9.0°, and at a 8.0 mm starting wall the material has to flow inward rather than be cut away.
Force is driven by the 655 MPa yield, the 8.0 mm wall and the 37.6 per cent reduction. One bite means 1,004 kN; with 3 passes the die sees around 394 kN.
Tip wall and springback on this part
Constant volume puts the wall at the small end near 10.13 mm, 27 per cent heavier than the 8.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.
Measure the cold part: recovery on this grade is about 0.26 mm on diameter and ovality near 1.3 per cent. Ring-gauge at a fixed distance from the end every time.
How 4140 chromoly behaves at 50 mm outside diameter
Supplied usually as quenched and tempered, which is exactly the wrong condition for cold forming. Either form it in the annealed state and harden afterwards, or expect a very narrow process window.
Inspection on a tapered part fails when it is done at the wrong moment with the wrong tool. A plan is three decisions: what, how often, and with what.
At 655 MPa yield with low ductility, this grade needs 3 passes on this geometry. The die is expected to last 9,811 pieces before the first re-polish, and the stress-relief practice is: Anneal before forming; quench and temper after. Cold forming Q&T stock is a scrap generator.
Typical applications are heavy shafts, gear blanks, die holders. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.
Cycle, tooling and piece cost
Cycle time is about 14.8 seconds from tube in to tube out, which is roughly 1,595 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 9,811 pieces before the first re-polish.
At the current price band the formed part costs about 3.25 USD, of which roughly 83 per cent is the blank. The recommended class is the Ø50 class (manual or automatic); a larger frame buys stiffness this diameter does not use.
How to quote this geometry
A readable drawing with OD, tip, cone length, wall and grade is enough for a first quote. Add the downstream operation so the allowance and the stress relief are specified rather than assumed.
For Chromoly 4140 (42CrMo / 40KhM) the decision that moves the number most is dimensional inspection plan. Say what you need there before asking for a price.
Frequently asked questions
What machine class forms a 50 → 31 mm tube?
The Ø50 class (manual or automatic). Forming force is about 394 kN per bite with 3 passes, so a smaller frame will deflect before it stalls.
How much thicker is the tip?
From 8.0 mm to about 10.13 mm, an increase of 27 per cent. Machine the bore after forming if the fit is tight.
What should I put on the drawing?
The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.26 mm on the die.
Talk to an engineer on WhatsApp
Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.
Chat on WhatsApp