What a 55 → 34 mm taper asks of the die

This geometry removes 37.5 per cent from the outside diameter over a 120 mm cone. The included cone angle is 9.8°, and at a 1.2 mm starting wall the material has to flow inward rather than be cut away.

The raw estimate is 59 kN for one bite. Split into 2 passes it becomes about 33 kN per bite, and the difference is the whole reason to plan the passes before choosing a press.

Tip wall and springback on this part

Constant volume puts the wall at the small end near 1.52 mm, 26 per cent heavier than the 1.2 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.

The tip comes back 0.037 mm larger than the die once the load is released. Ovality around 1.8 per cent is normal and is held down by a full-length guide bushing.

How carbon steel behaves at 55 mm outside diameter

Mild carbon steel is the reference material for taper forming: yield around 235 MPa, elongation above 25 %, and almost no springback surprise. Most dies are proved on it before anything harder is attempted.

Where the drawing calls for a thread, a face or a bore, the die has to leave stock. Too little and the thread runs out; too much and forming stops being competitive with machining.

At 235 MPa yield with high ductility, this grade needs 2 passes on this geometry. The die is expected to last 25,000 pieces before the first re-polish, and the stress-relief practice is: No heat treatment needed unless the part is fatigue-loaded; a 550–600 °C stress relief removes the formed-in stress.

Typical applications are lighting poles, guardrail posts, greenhouse hoops, general fabrication. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.

Cycle, tooling and piece cost

Cycle time is about 12.3 seconds from tube in to tube out, which is roughly 1,920 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 25,000 pieces before the first re-polish.

Raw material is 60 per cent of the 0.51 USD piece cost here. That ratio is why the L-120×400 F and not a heavier frame is the economic choice at this diameter.

How to quote this geometry

Send the two diameters, the cone length, the wall and the grade. State what you need on machining allowance after forming before asking for a price, because that decision drives the tooling.

For Carbon steel (St37 / Q235B) the decision that moves the number most is machining allowance after forming. Say what you need there before asking for a price.

Frequently asked questions

What machine class forms a 55 → 34 mm tube?

The L-120×400 F. Forming force is about 33 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.

How much thicker is the tip?

From 1.2 mm to about 1.52 mm, an increase of 26 per cent. Machine the bore after forming if the fit is tight.

What should I put on the drawing?

The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.037 mm on the die.