What a 55 → 34 mm taper asks of the die

This geometry removes 37.5 per cent from the outside diameter over a 120 mm cone. The included cone angle is 9.8°, and at a 4.0 mm starting wall the material has to flow inward rather than be cut away.

If this cone were formed in one stroke the die would take 181 kN. Our schedule uses 2 passes, bringing the per-bite load to 100 kN and leaving margin on the frame.

Tip wall and springback on this part

Constant volume puts the wall at the small end near 5.06 mm, 26 per cent heavier than the 4.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.

Elastic recovery adds about 0.064 mm to the tip diameter and typical ovality is 1.1 per cent. Compensate the recovery in the die rather than with the machine stop.

How 304 stainless behaves at 55 mm outside diameter

Low yield but severe work hardening: the cone gets hard as it forms, so the die load climbs through the stroke. Galling is the main risk and it is a lubrication problem before it is a die problem.

Changeover time decides the minimum batch size that is worth running. Below that number, the honest answer is to quote higher or decline.

At 215 MPa yield with medium ductility, this grade needs 2 passes on this geometry. The die is expected to last 17,502 pieces before the first re-polish, and the stress-relief practice is: Solution anneal if deformation exceeds about 15 %, otherwise corrosion resistance in the cone drops.

Typical applications are food equipment, architectural tube, exhaust tips. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.

Cycle, tooling and piece cost

Cycle time is about 12.3 seconds from tube in to tube out, which is roughly 1,920 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 17,502 pieces before the first re-polish.

Budget 3.48 USD per formed piece. Metal accounts for about 89 per cent of that, so the L-120×400 F is the sensible class rather than the next size up.

How to quote this geometry

If your part sits between two standard families, this page is the exact version and the case library is the decision matrix. Send either one with your quantity.

For Stainless 304 (08Kh18N10) the decision that moves the number most is changeover economics. Say what you need there before asking for a price.

Frequently asked questions

What machine class forms a 55 → 34 mm tube?

The L-120×400 F. Forming force is about 100 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.

How much thicker is the tip?

From 4.0 mm to about 5.06 mm, an increase of 26 per cent. Machine the bore after forming if the fit is tight.

What should I put on the drawing?

The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.064 mm on the die.

Talk to an engineer on WhatsApp

Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.

Chat on WhatsApp