What a 60 → 38 mm taper asks of the die

This geometry removes 37.5 per cent from the outside diameter over a 190 mm cone. The included cone angle is 6.8°, and at a 1.2 mm starting wall the material has to flow inward rather than be cut away.

If this cone were formed in one stroke the die would take 56 kN. Our schedule uses 2 passes, bringing the per-bite load to 31 kN and leaving margin on the frame.

Tip wall and springback on this part

Constant volume puts the wall at the small end near 1.52 mm, 26 per cent heavier than the 1.2 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.

Elastic recovery adds about 0.046 mm to the tip diameter and typical ovality is 1.8 per cent. Compensate the recovery in the die rather than with the machine stop.

How 316L stainless behaves at 60 mm outside diameter

Softer than 304 at the start and just as eager to work-harden. Molybdenum makes it galling-prone in a different way: it welds to the die rather than scratching it.

A cycle time is a promise about capacity. Quoting the fastest stroke instead of the average cycle is how a shift plan fails in the second week.

At 205 MPa yield with medium ductility, this grade needs 2 passes on this geometry. The die is expected to last 8,346 pieces before the first re-polish, and the stress-relief practice is: Anneal after heavy deformation; low carbon means no sensitisation risk at the weld.

Typical applications are chemical plant, marine hardware, medical frames. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.

Cycle, tooling and piece cost

Cycle time is about 14.3 seconds from tube in to tube out, which is roughly 1,651 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 8,346 pieces before the first re-polish.

Budget 2.69 USD per formed piece. Metal accounts for about 64 per cent of that, so the L-120×400 F is the sensible class rather than the next size up.

How to quote this geometry

If your part sits between two standard families, this page is the exact version and the case library is the decision matrix. Send either one with your quantity.

For Stainless 316L (03Kh17N14M2) the decision that moves the number most is cycle time planning. Say what you need there before asking for a price.

Frequently asked questions

What machine class forms a 60 → 38 mm tube?

The L-120×400 F. Forming force is about 31 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.

How much thicker is the tip?

From 1.2 mm to about 1.52 mm, an increase of 26 per cent. Machine the bore after forming if the fit is tight.

What should I put on the drawing?

The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.046 mm on the die.

Talk to an engineer on WhatsApp

Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.