What a 70 → 44 mm taper asks of the die
This geometry removes 37.4 per cent from the outside diameter over a 190 mm cone. The included cone angle is 7.9°, and at a 1.5 mm starting wall the material has to flow inward rather than be cut away.
The raw estimate is 86 kN for one bite. Split into 2 passes it becomes about 48 kN per bite, and the difference is the whole reason to plan the passes before choosing a press.
Tip wall and springback on this part
Constant volume puts the wall at the small end near 1.90 mm, 26 per cent heavier than the 1.5 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.
The tip comes back 0.057 mm larger than the die once the load is released. Ovality around 1.6 per cent is normal and is held down by a full-length guide bushing.
How 304 stainless behaves at 70 mm outside diameter
Low yield but severe work hardening: the cone gets hard as it forms, so the die load climbs through the stroke. Galling is the main risk and it is a lubrication problem before it is a die problem.
Cold forming gives a clean surface and cold-work strength. Hot forming buys reduction capacity and pays for it in scale, distortion and energy. The crossover is specific to wall and material.
At 215 MPa yield with medium ductility, this grade needs 2 passes on this geometry. The die is expected to last 8,401 pieces before the first re-polish, and the stress-relief practice is: Solution anneal if deformation exceeds about 15 %, otherwise corrosion resistance in the cone drops.
Typical applications are food equipment, architectural tube, exhaust tips. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.
Cycle, tooling and piece cost
Cycle time is about 14.7 seconds from tube in to tube out, which is roughly 1,606 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 8,401 pieces before the first re-polish.
Raw material is 71 per cent of the 3.21 USD piece cost here. That ratio is why the L-120×400 F and not a heavier frame is the economic choice at this diameter.
How to quote this geometry
Send the two diameters, the cone length, the wall and the grade. State what you need on hot or cold forming before asking for a price, because that decision drives the tooling.
For Stainless 304 (08Kh18N10) the decision that moves the number most is hot or cold forming. Say what you need there before asking for a price.
Frequently asked questions
What machine class forms a 70 → 44 mm tube?
The L-120×400 F. Forming force is about 48 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.
How much thicker is the tip?
From 1.5 mm to about 1.90 mm, an increase of 26 per cent. Machine the bore after forming if the fit is tight.
What should I put on the drawing?
The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.057 mm on the die.