What a 76 → 48 mm taper asks of the die
This geometry removes 37.5 per cent from the outside diameter over a 190 mm cone. The included cone angle is 8.6°, and at a 1.2 mm starting wall the material has to flow inward rather than be cut away.
A single full-reduction bite would need about 85 kN. The working schedule is 2 passes, which puts roughly 47 kN on the die each bite. That is the figure to size the machine and the tooling with.
Tip wall and springback on this part
Constant volume puts the wall at the small end near 1.52 mm, 26 per cent heavier than the 1.2 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.
Plan 0.051 mm of springback on the tip and roughly 1.8 per cent ovality. Both are cut into the tool geometry, not chased with the stroke setting after the parts drift.
How steel 20 behaves at 76 mm outside diameter
A step up in carbon from St37 with the same forming behaviour. The extra 0.08 % carbon raises strength after cold work but still leaves enough ductility for a single-pass cone.
Inspection on a tapered part fails when it is done at the wrong moment with the wrong tool. A plan is three decisions: what, how often, and with what.
At 245 MPa yield with high ductility, this grade needs 2 passes on this geometry. The die is expected to last 11,498 pieces before the first re-polish, and the stress-relief practice is: Normalise only if the part is welded afterwards or needs dimensional stability in service.
Typical applications are shafts, bushes, fork blanks, ground screw tips. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.
Cycle, tooling and piece cost
Cycle time is about 14.9 seconds from tube in to tube out, which is roughly 1,584 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 11,498 pieces before the first re-polish.
The piece cost lands near 1.20 USD with 55 per cent in the blank. Die amortisation is spread over 11,498 pieces before the first re-polish.
How to quote this geometry
Give us the five numbers and the grade, then ask for the first article as a named milestone. The 1.20 USD piece cost on this page is the planning baseline for it.
For Carbon steel 20 (AISI 1020) the decision that moves the number most is dimensional inspection plan. Say what you need there before asking for a price.
Frequently asked questions
What machine class forms a 76 → 48 mm tube?
The L-120×400 F. Forming force is about 47 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.
How much thicker is the tip?
From 1.2 mm to about 1.52 mm, an increase of 26 per cent. Machine the bore after forming if the fit is tight.
What should I put on the drawing?
The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.051 mm on the die.