What a 76 → 48 mm taper asks of the die
This geometry removes 37.5 per cent from the outside diameter over a 190 mm cone. The included cone angle is 8.6°, and at a 1.5 mm starting wall the material has to flow inward rather than be cut away.
If this cone were formed in one stroke the die would take 286 kN. Our schedule uses 3 passes, bringing the per-bite load to 112 kN and leaving margin on the frame.
Tip wall and springback on this part
Constant volume puts the wall at the small end near 1.90 mm, 26 per cent heavier than the 1.5 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.
Elastic recovery adds about 0.18 mm to the tip diameter and typical ovality is 1.9 per cent. Compensate the recovery in the die rather than with the machine stop.
How 4140 chromoly behaves at 76 mm outside diameter
Supplied usually as quenched and tempered, which is exactly the wrong condition for cold forming. Either form it in the annealed state and harden afterwards, or expect a very narrow process window.
The cone is the most precise surface on the part and the first thing to touch something hard. Handling damage is cheap to prevent and impossible to argue about after delivery.
At 655 MPa yield with low ductility, this grade needs 3 passes on this geometry. The die is expected to last 4,709 pieces before the first re-polish, and the stress-relief practice is: Anneal before forming; quench and temper after. Cold forming Q&T stock is a scrap generator.
Typical applications are heavy shafts, gear blanks, die holders. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.
Cycle, tooling and piece cost
Cycle time is about 42.2 seconds from tube in to tube out, which is roughly 559 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 4,709 pieces before the first re-polish.
Budget 3.37 USD per formed piece. Metal accounts for about 41 per cent of that, so the L-120×400 F is the sensible class rather than the next size up.
How to quote this geometry
If your part sits between two standard families, this page is the exact version and the case library is the decision matrix. Send either one with your quantity.
For Chromoly 4140 (42CrMo / 40KhM) the decision that moves the number most is packing formed ends. Say what you need there before asking for a price.
Frequently asked questions
What machine class forms a 76 → 48 mm tube?
The L-120×400 F. Forming force is about 112 kN per bite with 3 passes, so a smaller frame will deflect before it stalls.
How much thicker is the tip?
From 1.5 mm to about 1.90 mm, an increase of 26 per cent. Machine the bore after forming if the fit is tight.
What should I put on the drawing?
The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.18 mm on the die.
Talk to an engineer on WhatsApp
Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.
Chat on WhatsApp