What a 89 → 56 mm taper asks of the die
This geometry removes 37.5 per cent from the outside diameter over a 250 mm cone. The included cone angle is 7.6°, and at a 1.5 mm starting wall the material has to flow inward rather than be cut away.
A single full-reduction bite would need about 335 kN. The working schedule is 3 passes, which puts roughly 132 kN on the die each bite. That is the figure to size the machine and the tooling with.
Tip wall and springback on this part
Constant volume puts the wall at the small end near 1.90 mm, 27 per cent heavier than the 1.5 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.
Plan 0.21 mm of springback on the tip and roughly 1.9 per cent ovality. Both are cut into the tool geometry, not chased with the stroke setting after the parts drift.
How 4140 chromoly behaves at 89 mm outside diameter
Supplied usually as quenched and tempered, which is exactly the wrong condition for cold forming. Either form it in the annealed state and harden afterwards, or expect a very narrow process window.
Changeover time decides the minimum batch size that is worth running. Below that number, the honest answer is to quote higher or decline.
At 655 MPa yield with low ductility, this grade needs 3 passes on this geometry. The die is expected to last 2,747 pieces before the first re-polish, and the stress-relief practice is: Anneal before forming; quench and temper after. Cold forming Q&T stock is a scrap generator.
Typical applications are heavy shafts, gear blanks, die holders. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.
Cycle, tooling and piece cost
Cycle time is about 48.3 seconds from tube in to tube out, which is roughly 488 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 2,747 pieces before the first re-polish.
The piece cost lands near 6.40 USD with 32 per cent in the blank. Die amortisation is spread over 2,747 pieces before the first re-polish.
How to quote this geometry
Give us the five numbers and the grade, then ask for the first article as a named milestone. The 6.40 USD piece cost on this page is the planning baseline for it.
For Chromoly 4140 (42CrMo / 40KhM) the decision that moves the number most is changeover economics. Say what you need there before asking for a price.
Frequently asked questions
What machine class forms a 89 → 56 mm tube?
The L-120×400 F. Forming force is about 132 kN per bite with 3 passes, so a smaller frame will deflect before it stalls.
How much thicker is the tip?
From 1.5 mm to about 1.90 mm, an increase of 27 per cent. Machine the bore after forming if the fit is tight.
What should I put on the drawing?
The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.21 mm on the die.