What a 89 → 60 mm taper asks of the die

This geometry removes 32.6 per cent from the outside diameter over a 250 mm cone. The included cone angle is 6.6°, and at a 4.0 mm starting wall the material has to flow inward rather than be cut away.

A single full-reduction bite would need about 272 kN. The working schedule is 2 passes, which puts roughly 151 kN on the die each bite. That is the figure to size the machine and the tooling with.

Tip wall and springback on this part

Constant volume puts the wall at the small end near 4.87 mm, 22 per cent heavier than the 4.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.

Plan 0.091 mm of springback on the tip and roughly 1.0 per cent ovality. Both are cut into the tool geometry, not chased with the stroke setting after the parts drift.

How 304 stainless behaves at 89 mm outside diameter

Low yield but severe work hardening: the cone gets hard as it forms, so the die load climbs through the stroke. Galling is the main risk and it is a lubrication problem before it is a die problem.

A wrinkle is a stability failure: the wall buckles in compression before it can thicken. Adding force makes it worse, which is why every instinct at the machine is wrong here.

At 215 MPa yield with medium ductility, this grade needs 2 passes on this geometry. The die is expected to last 4,901 pieces before the first re-polish, and the stress-relief practice is: Solution anneal if deformation exceeds about 15 %, otherwise corrosion resistance in the cone drops.

Typical applications are food equipment, architectural tube, exhaust tips. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.

Cycle, tooling and piece cost

Cycle time is about 17.2 seconds from tube in to tube out, which is roughly 1,373 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 4,901 pieces before the first re-polish.

The piece cost lands near 12.07 USD with 80 per cent in the blank. Die amortisation is spread over 4,901 pieces before the first re-polish.

How to quote this geometry

Give us the five numbers and the grade, then ask for the first article as a named milestone. The 12.07 USD piece cost on this page is the planning baseline for it.

For Stainless 304 (08Kh18N10) the decision that moves the number most is wrinkling on thin wall. Say what you need there before asking for a price.

Frequently asked questions

What machine class forms a 89 → 60 mm tube?

The L-120×400 F. Forming force is about 151 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.

How much thicker is the tip?

From 4.0 mm to about 4.87 mm, an increase of 22 per cent. Machine the bore after forming if the fit is tight.

What should I put on the drawing?

The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.091 mm on the die.

Talk to an engineer on WhatsApp

Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.

Chat on WhatsApp