What machining allowance after forming means at 60 → 38 mm

Short version for Chromoly 4140 (42CrMo / 40KhM) at 60 → 38 mm: 0.93 mm of radial stock left on the cone for the finishing cut, which is cheaper than holding the formed diameter tighter than the process can. It is worth knowing why before you accept it, because the same three inputs that produce this answer will produce a different one the moment the wall or the grade changes.

Where the drawing calls for a thread, a face or a bore, the die has to leave stock. Too little and the thread runs out; too much and forming stops being competitive with machining.

How much stock, and where

On the outside diameter, 1.5–2 mm on diameter is the usual allowance to clean up die marks and ovality in one pass. On the tip face, 0.5–1 mm, because forming leaves the face slightly dished and not square to the axis. Budget 1.34 USD per piece at this combination, of which 79 per cent is metal.

On a bore, 1 mm on radius. Forming thickens the wall inward, so the bore is smaller and uneven; drilling from the formed surface without stock is how a bore ends up off-centre by 0.3 mm. Springback adds 0.17 mm to the tip diameter, so the die is cut that much under nominal.

The fixturing question behind the tolerance

Concentricity between the thread and the tube axis is set by how the part is held, not by how well it was formed. Chucking on the straight tube with a live centre in the cone gives the best result; chucking on the cone and hoping the jaw finds the axis does not. 15,698 pieces per die set is the working number here; below 7,849 pieces a year the tooling never pays back.

If concentricity is a real requirement, say it in the RFQ. It changes the process plan, the fixture and the price, and it is much cheaper to hear before the die is cut. The 3.7 per cent scrap allowance is not padding — it is the pass count and the material talking.

The numbers for this combination

Tube outside diameter60 mm
Small-end diameter38 mm
Wall thickness2.5 mm
Cone length95 mm
Reduction on diameter36.7 per cent
Half angle / included angle6.60° / 13.2°
Yield strength used655 MPa
Forming force, single bite371 kN
Forming force, per bite at 3 passes146 kN
Passes3 passes
Processcold forming
Cycle time15.5 s
Output per 8 h shift1,523 pieces
Tip wall after forming3.14 mm (+26 per cent)
Springback on tip diameter0.17 mm
Ovality at the tip1.6 per cent
Blank length171 mm
Blank weight0.606 kg
Machine classL-120×400 F

Computed for this combination. Confirm the force and the tip wall on a sample before the die is cut.

The force figure is the one people misread. 371 kN is what a single bite taking the whole 36.7 per cent reduction would need; the press in the schedule only sees 146 kN because the reduction is split. Quoting the first number for a multi-pass job is how machines get bought one size too large.

Read the table before the prose if you are in a hurry. The table is the part you can defend in a meeting; the prose explains which entries are sensitive to the material certificate and which are not.

How Chromoly 4140 (42CrMo / 40KhM) behaves at 36.7 per cent reduction

Supplied usually as quenched and tempered, which is exactly the wrong condition for cold forming. Either form it in the annealed state and harden afterwards, or expect a very narrow process window.

Chromoly 4140 (42CrMo / 40KhM) at this reduction behaves like a demanding material, and the schedule above is written for that. Push the reduction per pass and the failure mode is a longitudinal split starting at the tip edge, not a slow drift out of tolerance.

Typical use for this grade is heavy shafts, gear blanks, die holders. If your part sits outside that list, the numbers still apply but the corrosion and fatigue assumptions behind them do not.

Medium section: 60 → 38 mm

The 60 to 38 pair is the workhorse of the trade: fork blanks, furniture legs, pole sections. Tonnage is moderate and almost every machine size can do it, so the decision usually turns on cycle time and die life.

At 60 mm the guide bushing matters as much as the die. A 60 mm tube has enough length to lever against the die entry if the bushing clearance is loose, and the symptom is ovality at the tip that looks like a die problem and is not.

Floor space and power follow the class, not the part: a L-120×400 F needs the footprint in its own datasheet whether you run 60 mm or something smaller in it.

Cost per 1,000 pieces

Metal in the blank0.606 kg, 1.061 USD
Machine time15.5 s, 0.103 USD
Die cost, one set2,030 USD
Die life15,698 pieces
Scrap allowance3.7 per cent
Cost per piece1.34 USD
Cost per 1,0001,343 USD

Scrap is priced into 1.34 USD at 3.7 per cent. If your first article runs clean, the real cost is lower than this; if it does not, this number was optimistic and the difference shows up as a month of rework.

What to put on the drawing

Say what happens after forming: machined, welded, coated, or used as formed. The allowance, the stress relief and the surface spec all follow from that one line.

Add the as-formed wall at the tip as a reference dimension with a minimum. It is the dimension that decides whether the mating bore cleans up, and it is the one most often left off.

Send the drawing as a PDF with the dimensions readable at 100 per cent. Half the quotation delays we see come from a photo of a printout, not from a hard part.

Frequently asked questions

Can the die form to finished thread diameter?

Close, but the thread itself is cut or rolled. Forming to finish leaves no clean-up stock and the rolled thread inherits every die mark.

How much wall for an M36 thread on a 38 mm tip?

About 1 mm per side, so a 34 mm bore before threading. Check the actual formed section first, because the tip wall is thicker than nominal.

Does machining after forming cost much?

It is a second operation with a second setup. On high volume, forming closer to net shape and cutting only the thread is usually cheaper.

Is 4140 chromoly suitable for a part that will be welded after forming?

It welds, but the formed tip is work-hardened and the weld pool will dilute that. For a structural weld, stress relieve at 620 °C first, or move the weld away from the cone.

Would a smaller machine do this job?

Not at 146 kN per bite with a 60 mm tube to guide. The L-120×400 F is the smallest class that holds the die squarely at this diameter; a lighter frame deflects and the ovality shows up before the force limit does.

Talk to an engineer on WhatsApp

Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.

Chat on WhatsApp