What a 50 → 32 mm taper asks of the die

This geometry removes 36.0 per cent from the outside diameter over a 120 mm cone. The included cone angle is 8.6°, and at a 2.0 mm starting wall the material has to flow inward rather than be cut away.

The raw estimate is 133 kN for one bite. Split into 2 passes it becomes about 74 kN per bite, and the difference is the whole reason to plan the passes before choosing a press.

Tip wall and springback on this part

Constant volume puts the wall at the small end near 2.50 mm, 25 per cent heavier than the 2.0 mm blank. If the mating bore was dimensioned from the starting wall, it will not assemble. Add the as-formed tip wall to the drawing as a reference dimension with a minimum.

The tip comes back 0.069 mm larger than the die once the load is released. Ovality around 1.4 per cent is normal and is held down by a full-length guide bushing.

How steel 45 behaves at 50 mm outside diameter

Medium carbon: noticeably stronger, noticeably less forgiving. Springback is 30–40 % higher than mild steel, and the tip crack window narrows because the material has less elongation left before the die touches it.

A bad cone is not automatically scrap, and rework is not automatically cheaper. Three questions settle it: is the wall cracked, how much length is left, and what has already been spent on the part.

At 355 MPa yield with medium ductility, this grade needs 2 passes on this geometry. The die is expected to last 17,326 pieces before the first re-polish, and the stress-relief practice is: Normalise after forming whenever the part sees bending or cyclic load.

Typical applications are shafts, spindles, load-bearing pins. If your part sits outside that list, the forming numbers still apply but the corrosion and fatigue assumptions may not.

Cycle, tooling and piece cost

Cycle time is about 11.9 seconds from tube in to tube out, which is roughly 1,984 pieces in an eight-hour shift at 82 per cent utilisation. The die is expected to make 17,326 pieces before the first re-polish.

Raw material is 64 per cent of the 0.75 USD piece cost here. That ratio is why the Ø50 class (manual or automatic) and not a heavier frame is the economic choice at this diameter.

How to quote this geometry

Send the two diameters, the cone length, the wall and the grade. State what you need on scrap or rework before asking for a price, because that decision drives the tooling.

For Carbon steel 45 (AISI 1045) the decision that moves the number most is scrap or rework. Say what you need there before asking for a price.

Frequently asked questions

What machine class forms a 50 → 32 mm tube?

The Ø50 class (manual or automatic). Forming force is about 74 kN per bite with 2 passes, so a smaller frame will deflect before it stalls.

How much thicker is the tip?

From 2.0 mm to about 2.50 mm, an increase of 25 per cent. Machine the bore after forming if the fit is tight.

What should I put on the drawing?

The two diameters, cone length, wall, grade and the as-formed tip wall. Add springback compensation of about 0.069 mm on the die.

Talk to an engineer on WhatsApp

Send your tube drawing, material and target output. We will reply with a machine configuration, a measured sample plan and a factory quotation. WhatsApp +86 183 0020 2909 or email info@jixin.online.