32 to 23 mm Tube Taper, 4 mm Wall, 60 mm Long

Forming data for the 32 to 23 mm taper on 4 mm wall over 60 mm in 4130 chromoly: force 44.1 t, tip wall 4.8 mm, blank loss 52.4 mm, cycle 13.7 s, die angle 18.6 deg from the axis.

Geometry as drawn

Ø32Ø23taper 60 mm

Forming data

Tube OD32 mm
Finished tip23 mm
Parent wall4 mm
Wall at the tip (est.)4.8 mm
Taper length60 mm
Diameter reduction28.1 %
Forming force (est.)44.1 t
MachineL-120×400 F (Ø120 × 400 mm, semi-auto)
Die angle from axis18.6°
Blank length consumed52.4 mm
Cycle time (est.)13.7 s
Material4130 chromoly

What the numbers mean

A 28.1 percent diameter reduction puts this taper in the light band. The die does the work in the first two thirds of the stroke and the last third is calibration, which is why the tip diameter, not the flank, is what an operator adjusts.

The 4 mm parent wall finishes near 4.8 mm at the tip. That thickening is the reason a formed cone holds torque that a welded cone cannot: there is no seam and the grain follows the transition.

The cone consumes about 52.4 mm of tube, not the full 60 mm, because the wall grows as the diameter falls. Cut blanks to the naive length and the part finishes short by the difference.

Force at the end of the stroke is roughly 44.1 tonnes on this geometry and material, which is what sizes the press. The die is cut to 18.6 degrees from the axis to compensate springback.

Defects on this geometry

  • Crack at the tip — the reduction is high for this wall; open the die entry radius before adding force.
  • Wrinkling on the flank — thin wall with a short cone; slow the stroke or lengthen the taper.
  • Die marks and galling — thick wall raises contact pressure; polish the die and use EP lubricant.
  • Length drift — if the cone start point walks, measure the blanks before touching the die.

Material note

4130 chromoly runs at about 75 percent of the mild-steel stroke speed. Springback is about anneal after forming if the part is cycled, slow stroke degrees, so the die is cut under angle. Recommended: 4130 chromoly.

Quick answers

What forming force does a 32 to 23 mm taper need?

44.1 tonnes at the end of the stroke on 4130 chromoly, with a 4 mm wall over a 60 mm cone. That figure sizes the press: under 60 t runs on the L-120, up to 175 t on the L-200 CNC.

How much tube does this cone consume?

About 52.4 mm of the 60 mm cone, because the wall thickens as the diameter falls. Cut to the naive length and the part finishes short by roughly 7.6 mm.

Can it be formed in one pass?

Yes \u2014 one pass, no pre-heat. The diameter reduction here is 28.1 percent; above 45 percent on this wall we run two passes with an anneal between them.

What wall should I expect at the tip?

About 4.8 mm from a 4 mm parent wall, roughly 20 percent thicker. That thickening is why a formed cone takes torque a welded cone cannot.

Nearby specs

Where this geometry is used

32 mm tube covers most of what this machine family sees; the 32 to 23 mm taper is the pair we quote most often on that diameter.

Read the method behind these numbers: choosing the dimensions · cycle time by size · defect catalog · shop-floor clips

WhatsApp tiktok