89 to 49 mm Tube Taper, 2 mm Wall, 90 mm Long

Forming data for the 89 to 49 mm taper on 2 mm wall over 90 mm in 4130 chromoly: force 116.3 t, tip wall 2.6 mm, blank loss 71.8 mm, cycle 17.5 s, die angle 20.3 deg from the axis.

Geometry as drawn

Ø89Ø49taper 90 mm

Forming data

Tube OD89 mm
Finished tip49 mm
Parent wall2 mm
Wall at the tip (est.)2.6 mm
Taper length90 mm
Diameter reduction44.9 %
Forming force (est.)116.3 t
MachineL-120×400 F (Ø120 × 400 mm, semi-auto)
Die angle from axis20.3°
Blank length consumed71.8 mm
Cycle time (est.)17.5 s
Material4130 chromoly

What the numbers mean

A 44.9 percent diameter reduction puts this taper in the heavy band. The die does the work in the first two thirds of the stroke and the last third is calibration, which is why the tip diameter, not the flank, is what an operator adjusts.

The 2 mm parent wall finishes near 2.6 mm at the tip. That thickening is the reason a formed cone holds torque that a welded cone cannot: there is no seam and the grain follows the transition.

The cone consumes about 71.8 mm of tube, not the full 90 mm, because the wall grows as the diameter falls. Cut blanks to the naive length and the part finishes short by the difference.

Force at the end of the stroke is roughly 116.3 tonnes on this geometry and material, which is what sizes the press. The die is cut to 20.3 degrees from the axis to compensate springback.

Defects on this geometry

  • Crack at the tip — the reduction is high for this wall; open the die entry radius before adding force.
  • Wrinkling on the flank — thin wall with a short cone; slow the stroke or lengthen the taper.
  • Die marks and galling — thick wall raises contact pressure; polish the die and use EP lubricant.
  • Length drift — if the cone start point walks, measure the blanks before touching the die.

Material note

4130 chromoly runs at about 75 percent of the mild-steel stroke speed. Springback is about anneal after forming if the part is cycled, slow stroke degrees, so the die is cut under angle. Recommended: 4130 chromoly.

Quick answers

What forming force does a 89 to 49 mm taper need?

116.3 tonnes at the end of the stroke on 4130 chromoly, with a 2 mm wall over a 90 mm cone. That figure sizes the press: under 60 t runs on the L-120, up to 175 t on the L-200 CNC.

How much tube does this cone consume?

About 71.8 mm of the 90 mm cone, because the wall thickens as the diameter falls. Cut to the naive length and the part finishes short by roughly 18.2 mm.

Can it be formed in one pass?

Yes \u2014 one pass, no pre-heat. The diameter reduction here is 44.9 percent; above 45 percent on this wall we run two passes with an anneal between them.

What wall should I expect at the tip?

About 2.6 mm from a 2 mm parent wall, roughly 30 percent thicker. That thickening is why a formed cone takes torque a welded cone cannot.

Nearby specs

Where this geometry is used

89 mm tube covers most of what this machine family sees; the 89 to 49 mm taper is the pair we quote most often on that diameter.

Read the method behind these numbers: choosing the dimensions · cycle time by size · defect catalog · shop-floor clips